Interlloy Grade Nearest Related Specification Typical Composition (%) & Properties Description & Applications
C Mn Ph S Si
M1020 AS1443-M1020
BS970 PART 3 1991 070M20
(EN3B)
SAE/AISI 1020 GRADE 2
0.20 0.50 0.05
MAX
0.05
MAX
0.23 Mild steel for machined parts or shafting.
Can be case hardened and welds readily.

M1030 AS1443 - 1030
BS970 PART 3 1991 080M 30
(EN6A)
SAE/AISI 1030 GRADE 1
0.30 0.75 0.05
MAX
0.05
MAX
0.23 Medium high tensile steel for shafts and medium stressed parts.
Can be welded with care.
Can be heat treated.

1040* AS1443 - 1040
BS970 PART 1 1983 080M 40
(EN8)
SAE/AISI 1040 GRADE 1B
0.40 0.75 0.04
MAX
0.04
MAX
0.23 Medium high tensile steel for shafts and parts requiring 620MPa (40 tonne tensile).
Responds to heat treatment.

1045 AS1443 - 1045
BS970 PART 3 1991 080A47
(EN43B)
SAE/AISI 1045
0.45 0.75 0.04
MAX
0.04
MAX
0.23 Medium high tensile steel for shafts and machinery parts.
Suitable for induction and flame hardening.

 12L14 AS1443/ 12L14
BS970 230M07 leaded
(EN1A) Leaded
SAE/AISI 12L14
0.15 MAX 0.80 0.04 0.25 This premium grade of free cutting steel is used by repititon engineers ad general machining for a wide varitey of applications.

S1214 AS1443 - 1214
BS970 PART 3 1991 220M07
(EN1A)
SAE/AISI 1215
ESFC
0.15
MAX
1.00 0.09 0.35 0.15
MAX
For maximum machinability and free cutting properties.
Can be case hardened.